Ag
Al
B
Be
C
0.078
Cb
Cd
Co
Cr
12.3
Cu
0.07
Fe
Balance
Fm
H
La
Mg
Mn
0.43
Mo
0.01
N
Nb
Ni
0.13
O
O2
P
0.02
Pb
S
0.007
Si
0.38
Sn
Ta
Ti
U
V
Zn
Zr
Other Mercury Free Product | Made in India
Ferrite Content WRC Method = 5.4798 | Delong Method = 7.8141 | Schaffler Method = 7.8141
Physical Properties As Welded - Typical | HARDNESS (AS DEPOSITED) 34 Rc* (38-45 Rc)
Tensile Strength 89,700 PSI
Yield 78,500 PSI
Elongation 24%